MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Atom Adhesives AA-BOND 2113 Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: AA-BOND 2113 is a clear, low viscosity epoxy adhesive system that contains no solvents, cures at room temperature, has excellent flow ability and wetting characteristics, and adheres strongly to glass, ceramics, most metals and many plastics. AA-BOND 2113 is particularly recommended for assembly and repair work of fiber optic and other high performance electronic and aerospace systems and components, and for structural laminating applications where an initial low viscosity and near transparent "color" are needed. AA-BOND 2113 is a good electrical insulator, provides excellent resistance to weather, galvanic action, salt solutions and many other chemicals including mild acid and alkalis, petroleum solvents, lubricating oils, jet fuels and gasoline, and alcohol.

Appearance: Clear, transparent

Cure Type: Heat cure or Room Temperature

Benefits:

  • Good wetting
  • Solvent free
  • Excellent flowability
  • Adheres strongly to numerous substrates
Mix Ratio by weight: 100:11/Resin:Hardener

Substrates: Ceramics, glass to glass, fabrics, metals, laminates and other composite materials

Typical Application: assembly and repair work of fiber optic and other high performance electronic and aerospace systems and components structural laminating applications where an initial low viscosity and near transparent "color" are needed.

Information provided by Atom Adhesives

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/cc
Solids Content 100 %100 %
Viscosity 300 cP300 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8888
Adhesive Bond Strength 15.2 MPa2200 psi
Izod Impact, Notched 0.128 J/cm0.240 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 6.00e+13 ohm-cm6.00e+13 ohm-cm
Dielectric Constant 4.24.2
Dielectric Strength 16.1 kV/mm410 kV/in
Dissipation Factor 0.0200.020
 
Processing PropertiesMetricEnglishComments
Cure Time  240 min
@Temperature 65.0 °C
4.00 hour
@Temperature 149 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 30.0 min30.0 min
Shelf Life 12.0 Month12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zircar Zirconia ZOG Single Crystal Zirconia Grog Insulation
Borosilicate Glass

PATOM009 / 172324

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.