MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Specialty Suspension 471 PVC Homopolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Wire and Cable Grade

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Porosity 0.54 %
Viscosity Measurement 1.02PolyOne 1386; Inherent Viscosity; Internal Method
 2.37Correlation; Relative Viscosity
 
Descriptive Properties
Cell ClassificationGP-5-15443ASTM D1755
Dark Specks per 100 grams3Geon® 1217
Flow Time30 secGeon® 1169
FormsPowder
Generic NamePolyvinyl Chloride Homopolymer
Heat Loss, %0.08Bagged, Geon® 793
K-value70Correlation
Polymerization ProcessSuspension
Processing MethodExtrusion
 Injection Molding
QLC Gels0Geon® 1458
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
Residual Monomer0.1 ppmGeon® 1005
Sonic Sifter Particle Size0.008Retained on 40+60 Mesh, Geon® 812
 0.19Through 140 Mesh, Geon® 812
UsesInsulation
 Wire & Cable Applications

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Geon® Performance Solutions HC 2155 Polyvinyl Chloride, Flexible
Geon® Performance Solutions 210 Series 218 Polyvinyl Chloride Homopolymer (PVC Homopolymer)

PH1PN8218 / 102054

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.