MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

DuPont Mobility and Materials Crastin® T843FR BK851 PBTC-GF20FR(17)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled

Material Notes: 20% Glass Reinforced, Flame Retardant, Toughened, Polybutylene Terephthalate

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.59 g/cc0.0574 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0050 cm/cm0.0050 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.011 cm/cm0.011 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 87.0 MPa12600 psiISO 527-1/-2
Elongation at Break 4.0 %4.0 %ISO 527-1/-2
Tensile Modulus 5.80 GPa841 ksiISO 527-1/-2
Flexural Strength 142 MPa20600 psiISO 178
Poissons Ratio 0.350.35ISO 527-1/-2
Izod Impact, Notched (ISO) 8.00 kJ/m²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched 5.50 J/cm²
@Temperature 23.0 °C
26.2 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.900 J/cm²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 62631-3-1
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 62631-3-2
Dielectric Constant  4.7
@Frequency 1e+6 Hz
4.7
@Frequency 1e+6 Hz
IEC 62631-2-1
 5.2
@Frequency 100 Hz
5.2
@Frequency 100 Hz
IEC 62631-2-1
Dissipation Factor  0.0198
@Frequency 100 Hz
0.0198
@Frequency 100 Hz
IEC 62631-2-1
 0.0277
@Frequency 1e+6 Hz
0.0277
@Frequency 1e+6 Hz
IEC 62631-2-1
Comparative Tracking Index 225 V225 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 205 °C401 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 180 °C356 °FISO 75-1/-2
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
IEC 60695-11-10
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
IEC 60695-11-10
Oxygen Index 31 %31 %ISO 4589-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 °C482 °FInjection Optimum
 240 - 260 °C464 - 500 °FInjection
Mold Temperature 80.0 °C176 °FInjection Optimum
 30.0 - 130 °C86.0 - 266 °FInjection
Ejection Temperature 150 °C302 °F
Drying Temperature 120 °C248 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourDehumidified Dryer
Moisture Content 0.040 %0.040 %
Hold Pressure 60.0 MPa8700 psi
 
Descriptive Properties
AdditivesLubricants
Back pressureAs low as possible
Drying Recommendedyes
FMVSS ClassDNIISO 3795 (FMVSS 302)
Hold pressure time (s/mm)3
Part Marking CodePBTC-GF20FR(17)ISO 11469
ProcessingInjection Molding
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPBTC-GF20FR(17)ISO 1043

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSX5078 / 197718

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.