MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Master Bond EP41S-4 Chemically Resistant Two Component Epoxy System  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Discontinued product. Master Bond recommends EP41S-1HT as a replacement.

Master Bond Polymer System EP41S-1HT is a two component epoxy resin system designed for durable, high performance bonding, sealing, coating and encapsulating at high temperatures. EP41S-1HT is formulated to cure at ambient temperatures or more quickly at elevated temperatures. It withstands prolonged immersion in gasoline, gasohol, fuels, oils, alcohols, methyl, ethyl, butyl, ethyl acetates, toluene, as well as a wide number of other organic and inorganic solvents.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 3000 - 4000 cP
@Temperature 23.0 °C
3000 - 4000 cP
@Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 120 min
@Temperature 93.3 °C
1.00 - 2.00 hour
@Temperature 200 °F
 1440 min
@Temperature 23.0 °C
24.0 hour
@Temperature 73.4 °F
 
Descriptive Properties
Color Code"A" Black; "B" Clear
Mix Ratio by weight100/25
Set-Up Time, minutes15-20At Room Temperature

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMASTB054 / 52211

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.