Petrothene GA633050X01 is a linear low density polyethylene resin selected by customers for compounding and wire and cable applications. GA633050X01 is formulated without TNPP. Status: Developmental Availability: North America Application: Compounding; Wire & Cable Market: Compounding; Wire & Cable Processing Method: Compounding; Wire & Cable Information provided by LyondellBasell. |