MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Aremco-Bond™ 556-HT-UHC Electrically & Thermally Conductive Epoxy Adhesive, Silver-Filled, Highly Conductive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: Two-Part Epoxy Paste

Vendors: Aremco offers a broad line of electrically and thermally conductive adhesives and greases for applications from room temperature to 1700°F (927°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 3.70 g/cc
@Temperature 25.0 °C
3.70 g/cc
@Temperature 77.0 °F
mixed
Particle Size <= 20 µm<= 20 µm
Viscosity 40000 - 50000 cP40000 - 50000 cPMixed Viscosity at 25°C
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090
Shear Strength >= 6.89 MPa>= 1000 psiASTM D1002-9
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.00030 ohm-cm<= 0.00030 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 12.4 W/m-K86.1 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 199 °C390 °Fcontinuous
 249 °C480 °Fintermittent
 
Processing PropertiesMetricEnglishComments
Cure Time  15.0 min
@Temperature 149 °C
0.250 hour
@Temperature 300 °F
Alternative Cure B
 30.0 min
@Temperature 121 °C
0.500 hour
@Temperature 250 °F
Alternative Cure A
 120 min
@Temperature 79.4 °C
2.00 hour
@Temperature 175 °F
Recommended Cure
Pot Life >= 2880 min
@Temperature 25.0 °C
>= 2880 min
@Temperature 77.0 °F
25 g
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
ColorSilver
FillerSilver Flake
Mix Ratio by Weight100:2resin:hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAREM18c / 256044

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.