MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company ESD 4485 High Temperature Nylon (HTN); Carbon Fiber - ESD Protection - Electrically Conductive
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc1.30 g/ccASTM D 792
Additive Loading 30 %30 %Primary Additive
Linear Mold Shrinkage 0.00050 - 0.0015 cm/cm
@Thickness 3.20 mm
0.00050 - 0.0015 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 248 MPa36000 psiASTM D 638
Elongation at Break 1.5 - 2.0 %1.5 - 2.0 %ASTM D 638
Tensile Modulus 23.4 GPa3400 ksiASTM D 638
Flexural Strength 359 MPa52000 psiASTM D 790
Flexural Modulus 20.7 GPa3000 ksiASTM D 790
Izod Impact, Notched 0.694 J/cm
@Thickness 3.20 mm
1.30 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 6.94 J/cm
@Thickness 3.20 mm
13.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1000 ohm-cm<= 1000 ohm-cmASTM D 257
Surface Resistivity per Square <= 1e+05<= 1e+05ASTM D 257; ESD STM11.11
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 260 °C500 °FASTM D 648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 310 - 343 °C590 - 650 °F
Mold Temperature 135 - 163 °C275 - 325 °F
Drying Temperature 79.4 °C
@Time 14400 sec
175 °F
@Time 4.00 hour
Moisture Content 0.10 %0.10 %
Dew Point -40.0 °C-40.0 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman SCHULAMID® 66 PTFE20 HS 20% PTFE Lubricated, Heat Stabilized Nylon 6/6
RTP Company RTP 399 X 141353 EG Polycarbonate (PC); ESD Protection - Permanently Static Dissipative - Flame Retardant - Extrusion Grade - Preliminary Datasheet
RTP Company RTP 299 D X 130507 A Nylon 6/12 (PA); Flame Retardant - Halogen Free
RTP Company RTP 199 X 136882 C Polypropylene (PP); Permanently Static Dissipative - ESD Protection - UV Stabilized - Mineral - Preliminary
RTP Company RTP 1199 A X 136859 B EG Polyethylene Terephthalate Glycol Modified (PETG); Permanently Static Dissipative - Extrusion Grade - ESD Protection

PQZRA32544 / 205898

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.