MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 771.0-T52, Sand Cast
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium 771.0-T52; UNS A07710; AA771.0-T52; Al771.0-T52
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.81 g/cc0.102 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 70 - 10070 - 100AA; Typical; 500 g load; 10 mm ball
Hardness, Knoop 109109Estimated from Brinell Hardness.
Hardness, Rockwell A 3636Estimated from Brinell Hardness.
Hardness, Rockwell B 5353Estimated from Brinell Hardness.
Hardness, Vickers 9696Estimated from Brinell Hardness.
Tensile Strength, Ultimate >= 248 MPa>= 36000 psiAA
Tensile Strength, Yield >= 207 MPa
@Strain 0.2 %
>= 30000 psi
@Strain 0.2 %
AA
Elongation at Break >= 1.5 %>= 1.5 %AA; in 2 in. (50 mm) or 4D
Tensile Modulus 71.0 GPa10300 ksiCompressive modulus in is typically about 2% higher for Al alloys
Poissons Ratio 0.330.33Estimated from aluminum 770.0
Machinability 90 %90 %0-100 Scale (100=best)
Shear Modulus 26.5 GPa3840 ksiEstimated from aluminum 770.0
Shear Strength 151 MPa21900 psiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000460 ohm-cm0.00000460 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 389 J/g167 BTU/lbTypical for cast aluminum
CTE, linear  24.7 µm/m-°C
@Temperature 20.0 - 100 °C
13.7 µin/in-°F
@Temperature 68.0 - 212 °F
 26.6 µm/m-°C
@Temperature 20.0 - 300 °C
14.8 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.963 J/g-°C0.230 BTU/lb-°FTypical for cast aluminum
Thermal Conductivity 138 W/m-K958 BTU-in/hr-ft²-°F
Melting Point 604 - 643 °C1120 - 1190 °F
Solidus 604 °C1120 °F
Liquidus 643 °C1190 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 90.4 - 92.5 %90.4 - 92.5 %As remainder
Chromium, Cr 0.06 - 0.20 %0.06 - 0.20 %
Copper, Cu <= 0.10 %<= 0.10 %
Iron, Fe <= 0.15 %<= 0.15 %
Magnesium, Mg 0.80 - 1.0 %0.80 - 1.0 %
Manganese, Mn <= 0.10 %<= 0.10 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.15 %<= 0.15 %
Titanium, Ti 0.10 - 0.20 %0.10 - 0.20 %
Zinc, Zn 6.5 - 7.5 %6.5 - 7.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 6063-T5
Aluminum 771.0-T5, Sand Cast
Aluminum 771.0-T6, Sand Cast
Aluminum 771.0-T71, Sand Cast
Aluminum 851.0-T6, Permanent Mold Cast

MAC7710T52 / 10199

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.