MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Zircar Refractory Composites RSBD-HD ALUMINA-SILICA INSULATION
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: ZRCI Alumina-Silica Insulation Type RSBD-HD Board is a ceramic fiber insulation suitable for use to 1260°C (2300°C). It is a strong, rigid refractory structure of high temperature ceramic fibers and high purity inorganic binders. It offers low thermal conductivity, excellent thermal shock resistance and is an effective thermal insulator in numerous thermal process systems. It is also well-suited for applications experiencing vibration, mechanical stress and strong erosive forces. The excellent rigidity and modulus of rupture possessed by this board makes it strong and self-supporting, yet relatively lightweight and easy to cut or machine. This product's features allow for quick, efficient handling and high installation rates, thereby enabling fast turnaround times in a variety of industrial insulation applications. Once installed, it can help reduce energy costs and cycling times due to its high insulating capability, as well as serving to protect refractory surfaces from thermal shock. Type RSBD-HD Board exhibits excellent chemical stability, resisting attack by most corrosive agents. Exceptions are hydrofluoric, phosphoric, hydrochloric and sulfuric acids as well as concentrated alkalis. It will also resist oxidation and reduction to a certain point. If wet by water, steam or oil upon drying all properties will be restored.

Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.419 g/cc0.0151 lb/in³
Loss On Ignition 6.0 - 7.0 %6.0 - 7.0 %
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00210 GPa0.305 ksiparallel to thickness
 0.000870 GPa
@Temperature 1010 °C,
Time 86400 sec
0.126 ksi
@Temperature 1850 °F,
Time 24.0 hour
parallel to thickness
Compressive Yield Strength 0.240 MPa34.8 psiat 5% compression ,after 24 hrs at 1010°C, parallel to thickness
 0.400 MPa58.0 psiat 5% compression, parallel to thickness
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 1.06 kV/mm27.0 kV/in
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.110 W/m-K
@Temperature 204 °C
0.763 BTU-in/hr-ft²-°F
@Temperature 399 °F
 0.170 W/m-K
@Temperature 649 °C
1.18 BTU-in/hr-ft²-°F
@Temperature 1200 °F
 0.220 W/m-K
@Temperature 1010 °C
1.53 BTU-in/hr-ft²-°F
@Temperature 1850 °F
Maximum Service Temperature, Air 1260 °C2300 °F
Shrinkage <= 5.0 %
@Temperature 1200 °C,
Time 14400 sec
<= 5.0 %
@Temperature 2190 °F,
Time 4.00 hour
 
Component Elements PropertiesMetricEnglishComments
Al2O3 60 - 65 %60 - 65 %
SiO2 10 - 15 %10 - 15 %
 
Descriptive Properties
ColorWhite
Kaolin Clay, %15 to 20
Organic Content, %5 to 10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DWA 6091/SiC/20p-T6 Aluminum SiC Metal-Matrix-Composite (Al MMC)
Zircar Refractory Composites RS-99-45 Refractory Sheet
Zircar Refractory Composites RS-A3 Refractory Sheet
Zircar Refractory Composites RS-99-60 Refractory Sheet
DWA 2009/SiC/25p-T4 Aluminum SiC Metal-Matrix-Composite (Al MMC)

CZRCI41 / 2904

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.