MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Bond 970-3 Room Temperature Cure General Purpose Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: TRA-BOND 970-3 general purpose adhesive is a non-flowing blue paste. This adhesive cures at room temperature. This adhesive is available in kits with a mix ratio of 100 parts A to 74 parts B or premixed and frozen in convenient, disposable syringes.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 61000 cP61000 cPMixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7070
Adhesive Bond Strength 34.5 MPa5000 psiLap shear, alum to alum
 
Processing PropertiesMetricEnglishComments
Cure Time  120 min
@Temperature 70.0 °C
2.00 hour
@Temperature 158 °F
 2880 min
@Temperature 25.0 °C
48.0 hour
@Temperature 77.0 °F
Shelf Life 12.0 Month12.0 MonthIn kits @ 25°C
 6.00 Month
@Temperature -40.0 °C
6.00 Month
@Temperature -40.0 °F
PMF
 
Descriptive Properties
Color Blue
Working Life hours 1.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRAC214 / 71142

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.