MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Melos FM 0526 Special bedding compound
Categories: Polymer; Thermoplastic

Material Notes: Special bedding compound.

Compound class: Bedding compound

Based on: TPE-O

Characteristics: Halogen free flame retardant

Application examples: Insulation
2 XI 1; XLPE; acc. DIN / VDE 0207 part 22
2 YI 1 – 5; PE; acc. DIN / VDE 0207 part 2
9 YI 1; PP; acc. DIN / VDE 0207 part 7

Application examples: Sheathing
HM 4 – 2; HFFR; acc. DIN / VDE 0207 part 24
2 YM 3; HDPE; acc. DIN / VDE 0207 part 3

Typical applications: Bedding compound for cables and wire according to VDE 0472 part 814 with max. 90°C operating temperature at conductor

Features: For 2-step process(coilable); Flame retardant; Halogen-free

Information provided by Melos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0578 lb/in³pressed plaques, 100°C / 5 min.; DIN EN ISO 1183-1A
pH >= 4.3>= 4.3Corrosivity, pressed plaques, 100°C / 5 min.; IEC 60754-2, Annex A
Mooney Viscosity 35
@Temperature 100 °C
35
@Temperature 212 °F
ML (1+4); DIN ISO 289-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 3535pressed plaques, 100°C / 5 min.; DIN ISO 7619-1
Tensile Strength >= 4.00 MPa>= 580 psipressed plaques, 100°C / 5 min.; IEC 60811-501
Elongation at Break >= 300 %>= 300 %pressed plaques, 100°C / 5 min.; IEC 60811-501
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+10 ohm-cm
@Temperature 27.0 °C
>= 1.00e+10 ohm-cm
@Temperature 80.6 °F
VDE 0472 Part 503
Surface Resistance >= 1.00e+9 ohm
@Temperature 23.0 °C
>= 1.00e+9 ohm
@Temperature 73.4 °F
VDE 0472 Part 502
 
Processing PropertiesMetricEnglishComments
Processing Temperature 110 - 120 °C230 - 248 °FTool
 110 - 120 °C230 - 248 °FMaximum mass temperature
Zone 1 60.0 - 70.0 °C140 - 158 °F
Zone 2 70.0 - 80.0 °C158 - 176 °F
Zone 3 85.0 - 95.0 °C185 - 203 °F
Zone 4 95.0 - 105 °C203 - 221 °F
Adapter Temperature 105 - 115 °C221 - 239 °F
Head Temperature 110 - 120 °C230 - 248 °F
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) 34 %34 %pressed plaques, 100°C / 5 min.; ASTM D 2863 A
 
Descriptive Properties
Conductivity=100 µS/mmpressed plaques, 100°C / 5 min., IEC 60754-2
Screw60-70°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMELOS082 / 296189

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.