MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Epoxies, Etc 50-3152 FR Flame Retardant Thermally Conductive Epoxy Resin
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: 50-3152 FR Potting and Encapsulating Compound has been formulated to meet the stringent nonburning requirements of UL 94 V-0. 50-3152FR Epoxy is listed with Underwriter’s Laboratories for passing UL 94 V-0. It also has a Comparative Tracking Index (CTI) of >600 Volts (PLC 0). 50-3152 FR is a two component epoxy potting and encapsulating system. This semi-rigid epoxy has excellent shock and vibration resistance along with good thermal conductivity. 50-3152 FR is designed for ease of use. It has a convenient 1:1 mix ratio and is low in viscosity.

Features:

  • Thermally conductive
  • Easy 1:1 ratio
  • Shock and vibration resistant
Benefits:
  • Protects electronics by quickly transferring heat
  • Simple to use in production
  • Will not damage electronic components

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.49 g/cc1.49 g/ccHardener
 1.55 g/cc1.55 g/ccResin
Viscosity 20000 cP20000 cPResin
 31000 cP31000 cPMixed
 64000 cP64000 cPHardener
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D  50
@Temperature 65.0 °C
50
@Temperature 149 °F
 80
@Temperature 25.0 °C
80
@Temperature 77.0 °F
Compressive Strength 51.7 MPa7500 psi
Shear Strength 17.2 MPa2500 psiLap (Al to Al)
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 7.60e+13 ohm-cm7.60e+13 ohm-cm
Dielectric Constant 5.0
@Frequency 100 Hz
5.0
@Frequency 100 Hz
Dielectric Strength 15.7 kV/mm400 kV/in
Comparative Tracking Index 600 V600 V
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.01 W/m-K7.01 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 135 °C275 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  30.0 min
@Temperature 100 °C
0.500 hour
@Temperature 212 °F
 120 - 180 min
@Temperature 65.0 °C
2.00 - 3.00 hour
@Temperature 149 °F
 1440 - 2880 min
@Temperature 25.0 °C
24.0 - 48.0 hour
@Temperature 77.0 °F
Pot Life 100 min
@Load 0.100 kg
100 min
@Load 0.221 lb
 
Descriptive Properties
ColorBeigeHardener
 BlackMixed
 BlackResin

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFEPOX054 / 316731

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.