MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Vartega Fenix Fiber+™ Recycled Carbon Fiber
Categories: Carbon; Carbon Fiber/Carbon Fibre

Material Notes: Vartega® produces recycled carbon fiber in a chopped and oversized EasyFeed Bundle™ format, typically used to enhance the physical properties of thermoplastic compounds. Fibers are provided as densified, easy flow bundles, with fiber lengths available from 3 to 12mm.

Fenix Fiber Pro™ has better mechanical performance than Fenix Fiber™ and Fenix Fiber Pro™. It is composed of SM/IM fiber of mixed or known lineage, sized with MITO functionalized graphene.

Information provided by Vartega, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density >= 0.250 g/cc
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 270 °C
 
Descriptive Properties
Nominal Bundle Length24 mm
Nominal Fiber Length12 mm
Polymer compatibilityEpoxy (general purpose)
Sizing Composition1.5% Epoxy

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PVART992 / 319207

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.