MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Phillips 66 Paper Machine Oil ISO 320
Categories: Fluid; Lubricant

Material Notes: Paper Machine Oil is a high-quality circulating oil developed for use in modern papermaking machines. It is recommended for use in paper machines manufactured by all leading OEMs. It is specially formulated to provide excellent detergency for system cleanliness while still maintaining excellent water-separating properties. Paper Machine Oil is formulated with an additive package specially tailored for papermaking machines. It has good oxidation resistance and thermal stability at high temperatures to minimize deposit formation and provide long service life. It has excellent detergency to help maintain system cleanliness. It has excellent water-separating properties to minimize the formation of emulsions, and passes the Pall Filterability Test for both new oil and “aged” oil contaminated with water. It has good load-carrying capacity for wear protection, protects system components against rust and corrosion, and has good foam resistance.

Applications:

  • Circulating systems of paper machines, including wet-end systems, dryer sections and calendar stacks
  • Circulating systems for heavily loaded bearings where moisture contamination is a problem and operating temperatures are high
  • Reduction gears and gear-head motors
  • Vacuum pumps and water pumps
Features/Benefits:
  • Excellent detergency
  • Excellent water-separating properties
  • Excellent filterability for use with fine porosity filters
  • Good oxidation resistance and thermal stability
  • High load-carrying capacity
  • Protects against rust and corrosion
  • Good foam resistance

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.887 g/cc
Density 7.39 lb/gal
Viscosity Measurement 97Index
Saybolt Viscosity at 100°F 1704 SUS
Saybolt Viscosity at 210°F 121 SUS
Kinematic Viscosity at 40°C (104°F) 320 cSt
Kinematic Viscosity at 100°C (212°F) 24.4 cSt
ASTM Color 4.5ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.70[mg KOH/g]; ASTM D974
 
Mechanical PropertiesOriginal ValueComments
Timken Test 30.0 lbOK Load; ASTM D2509
 
Thermal PropertiesOriginal ValueComments
Pour Point -12.0 °C
Flash Point 270 °CCOC
 
Descriptive Properties
Copper Corrosion1aASTM D130
Demulsibility10 minutes to passASTM D1401

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5203 / 198456

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.