MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

CoorsTek EXYRA™ BULK YTTRIA Min. 99.9% Y2O3
Categories: Ceramic; Oxide

Material Notes:

Information provided by CoorsTek.

Key Words: Y2O3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.95 g/cc0.179 lb/in³ASTM-C20
Grain Size 30 µm30 µmASTM-E112
 10 - 70 µm10 - 70 µmASTM-E112
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers  6.0
@Load 1.00 kg
6.0
@Load 2.20 lb
ASTM-C1327
 7.0
@Load 0.500 kg
7.0
@Load 1.10 lb
ASTM-C1327
Modulus of Elasticity 170 GPa24700 ksiASTM-C848
Flexural Strength 100 MPa14500 psi4-Point; ASTM-C1161
 140 MPa20300 psi3-Point; ASTM-C1161
Poissons Ratio 0.280.28ASTM-C848
Fracture Toughness 1.20 MPa-m½1.09 ksi-in½KIC; KNOOP 1000 gm
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  400000 ohm-cm
@Temperature 1000 °C
400000 ohm-cm
@Temperature 1830 °F
ASTM-D1829
 1.00e+7 ohm-cm
@Temperature 600 °C
1.00e+7 ohm-cm
@Temperature 1110 °F
ASTM-D1829
 1.00e+9 ohm-cm
@Temperature 500 °C
1.00e+9 ohm-cm
@Temperature 932 °F
ASTM-D1829
 1.00e+12 ohm-cm
@Temperature 300 °C
1.00e+12 ohm-cm
@Temperature 572 °F
ASTM-D1829
 >= 1.00e+14 ohm-cm
@Temperature 25.0 °C
>= 1.00e+14 ohm-cm
@Temperature 77.0 °F
ASTM-D1829
Dielectric Constant  11.5
@Frequency 1e+6 Hz
11.5
@Frequency 1e+6 Hz
ASTM-D150
 11.5
@Frequency 5.00e+9 Hz
11.5
@Frequency 5.00e+9 Hz
TE011 Resonant Mode
Dielectric Strength 16.5 kV/mm
@Thickness 1.00 mm
420 kV/in
@Thickness 0.0394 in
ASTM-D116
Dissipation Factor <= 0.00010<= 0.00010ASTM-D150
 0.000015
@Frequency 5.00e+9 Hz
0.000015
@Frequency 5.00e+9 Hz
TE011 Resonant Mode
 
Thermal PropertiesMetricEnglishComments
CTE, linear  7.00 µm/m-°C
@Temperature 400 °C
3.89 µin/in-°F
@Temperature 752 °F
ASTM-C372
 7.70 µm/m-°C
@Temperature 800 °C
4.28 µin/in-°F
@Temperature 1470 °F
ASTM-C372
 7.90 µm/m-°C
@Temperature 1000 °C
4.39 µin/in-°F
@Temperature 1830 °F
ASTM-C372
Specific Heat Capacity 0.450 J/g-°C0.108 BTU/lb-°FASTM-E1269
Thermal Conductivity 15.0 W/m-K104 BTU-in/hr-ft²-°FASTM-C408
 
Component Elements PropertiesMetricEnglishComments
Iron, Fe <= 0.00020 %<= 0.00020 %in Sintered Material per Glow Discharge Mass Spec
Magnesium, Mg <= 0.00010 %<= 0.00010 %in Sintered Material per Glow Discharge Mass Spec
Other, total <= 0.050 %<= 0.050 %in Sintered Material per Glow Discharge Mass Spec
Silicon, Si <= 0.010 %<= 0.010 %in Sintered Material per Glow Discharge Mass Spec
Sodium, Na <= 0.00010 %<= 0.00010 %in Sintered Material per Glow Discharge Mass Spec
Y2O3 >= 99.9 %>= 99.9 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CCOOR825 / 254573

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.