MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Ineos L34N-00 Polypropylene Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Grade L34N-00 typically has a 35 melt flow rate and is a low gloss, high impact polypropylene copolymer. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.

Key Words: Low gloss, high impact
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.015 cm/cm0.015 in/inInjection Molded; ASTM D955
Linear Mold Shrinkage, Transverse 0.016 cm/cm0.016 in/inInjection Molded; ASTM D955
Melt Flow 34 g/10 min
@Load 2.16 kg,
Temperature 230 °C
34 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8989Injection Molded; ASTM D785
Tensile Strength at Break 19.2 MPa2790 psi2.0 in/min, Injection Molded; ASTM D638
Tensile Strength, Yield 26.9 MPa3900 psi2.0 in/min, Injection Molded; ASTM D638
Elongation at Break 130 %130 %2.0 in/min, Injection Molded; ASTM D638
Elongation at Yield 5.2 %5.2 %2.0 in/min, Injection Molded; ASTM D638
Flexural Modulus, 1% Secant 1190 MPa173000 psiInjection Molded; ASTM D790A
Izod Impact, Notched  0.641 J/cm
@Temperature -20.0 °C
1.20 ft-lb/in
@Temperature -4.00 °F
Injection Molded; ASTM D256
 1.49 J/cm
@Temperature 22.8 °C
2.80 ft-lb/in
@Temperature 73.0 °F
Injection Molded; ASTM D256
Impact  NB
@Temperature -20.0 °C
NB
@Temperature -4.00 °F
Instrument Dart Impact, Injection Molded, Ductile Failure; ASTM D3763
 NB
@Temperature 22.8 °C
NB
@Temperature 73.0 °F
Instrument Dart Impact, Injection Molded, Ductile Failure; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 106 °C223 °FUnannealed, Injection Molded; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 57.2 °C135 °FUnannealed, Injection Molded; ASTM D648
Vicat Softening Point 151 °C304 °FASTM D1525
Brittleness Temperature -30.0 - -20.0 °C-22.0 - -4.00 °FASTM D746
Flammability, UL94  HB
@Thickness 1.52 mm
HB
@Thickness 0.0600 in
NC
 HB
@Thickness 3.05 mm
HB
@Thickness 0.120 in
NC
 
Optical PropertiesMetricEnglishComments
Gloss 59 %59 %60°, Injection Molded; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
ProcessInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PINEOS903 / 104596

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.