MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Polynt DISTITRON® 459 AV4 Unsaturated Polyester Resin
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: Unsaturated polyester resin in styrene, Orthophthalic

Appearance: Neutral - Transparent

Main resin characteristics: Clear, unaccelerated, Light stabilized

Main applications: Flat sheets, laminates, Transparent and corrugated sheets

Curing cycle: 24h at 23°C + 2h at 100°C + 1h at 100°C

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³
Solids Content 65 - 67 %65 - 67 %MT-CU001C
Brookfield Viscosity 500 - 630 cP500 - 630 cPsp 2 rpm 20; MT-CU025V
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 4343ASTM D 2583
Tensile Strength 70.0 MPa10200 psiISO 527
Elongation at Break 2.3 %2.3 %ISO 527
Tensile Modulus 4.00 GPa580 ksiISO 527
Flexural Strength 130 MPa18900 psiISO 178
Flexural Modulus 3.90 GPa566 ksiISO 178
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C149 °FISO 75 -2A
 
Processing PropertiesMetricEnglishComments
Gel Time 18.0 - 22.0 min
@Temperature 25.0 °C
18.0 - 22.0 min
@Temperature 77.0 °F
Reactivity at 25°C + 0,2% Co 6% + 1% MEKP50; RS.08.G
Shelf Life 6.00 Month6.00 Monthin the dark; MT-CU002S
 
Descriptive Properties
Peak Exotherm140 - 170°CRS.08.G; Reactivity at 25°C + 0,2% Co 6% + 1% MEKP50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYN9411 / 232006

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.