MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Envalior Novamid® ID 1030-CF10 Nylon 6/66, 3D Printing Grade, 10% Carbon Reinforced
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66

Material Notes: This is a filament grade - not available for sale as granules.

Novamid® ID 1030-CF10 can 3D-print high-performance and durable structural end-use parts, making 3D printing technology a viable option for demanding automotive structural applications that require robust performance at elevated temperatures. With a carbon fiber loading of just 10%, Novamid® ID 1030-CF10 prints parts with properties close to what is usually achievable only by injection molding. It can be printed at the same speeds as unreinforced plastics, while achieving considerably better strength and toughness.

Processing technology: 3D printing

Data refer to dry testing conditions.

Former DSM Engineering Plastics product line is now with Envalior.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 58.0 MPa3D printed: flat Y-X direction; ISO 527-1/-2
 110 MPaISO 527-1/-2
 110 MPa3D printed: flat X-X direction; ISO 527-1/-2
Tensile Strength, Yield 63.0 MPa3D printed: flat Y-X direction; ISO 527-1/-2
 110 MPaISO 527-1/-2
 110 MPa3D printed: flat X-X direction; ISO 527-1/-2
Elongation at Break 2.2 %3D printed: flat X-X direction; ISO 527-1/-2
 3.0 %ISO 527-1/-2
 4.5 %3D printed: flat Y-X direction; ISO 527-1/-2
Elongation at Yield 2.5 %3D printed: flat X-X direction; ISO 527-1/-2
 2.8 %ISO 527-1/-2
 3.0 %3D printed: flat Y-X direction; ISO 527-1/-2
Tensile Modulus 2720 MPa3D printed: flat Y-X direction; ISO 527-1/-2
 7570 MPaISO 527-1/-2
 7630 MPa3D printed: flat X-X direction; ISO 527-1/-2
 
Thermal PropertiesOriginal ValueComments
Melting Point 200 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 184 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 153 °CISO 75-1/-2
Glass Transition Temp, Tg 58.0 °C10°C/min; ISO 11357-1/-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDSM7998 / 254063

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.