MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Thermoseal

Klinger Thermoseal Milam Mica PSS 300 Laminate
Categories: Ceramic; Oxide

Material Notes: Type PSS. High Quality Mica Sheet. Laminated on Pegged Stainless Steel Insert. All Milam laminates are suitable for use in hot, dry gas applications such as exhaust manifolds, turbines, turbo chargers and air heat exchangers.

Information provided by Thermoseal Inc.

Vendors: Thermoseal Inc. is the exclusive North American producer of Klinger Fluid Sealing products, including popular lines: Sealex, Klingersil and Topchem and our new Performance Technology Group of products. Visit us at Thermosealinc.com or call 1-800-990-7325 to speak with a fluid sealing specialist.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Thickness 3180 microns125 miltolerance +/- 5%
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air <= 900.0 °C<= 1652 °F
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) <= 15 %<= 15 %DIN 52911
 
Descriptive Properties
Colormetallic tan
Compressibility18-23%ASTM F36A
Gas LeakageDIN 3535/6
Recovery48-53%ASTM F36A
Sheet Size47in x 40 in
Stressmax. 11602 psi
Stress Relaxation2900 psi40 MPa, 300°C, DIN 52913
 4351 psi50MPa, 300°C, DIN 52913
Tang Insert Stainless Steel Thickness0.004" x2ASTM 316

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTHERM952 / 192640

Thermoseal

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.