MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Colmant Coated Fabrics AEM (VAMAC®) Coated Polyester Tire Cord
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Tire cord fabric is a type of industrial fabric which is constructed using High Tenacity yarns in the warp direction and yarns of negligible resistance in weft direction which is used to hold warn yarns locked in their position. Tire cord coated fabrics provides fundamental properties such as controlled deformation, high strength, abrasion resistance, etc. Widely used by the tire industry, it is also employed for the rubber hose manufacture, air springs, expansion joints, among many other applications. Polyester is a the synthetic fiber that detains the first place in terms of global production. It is a linear polymer whose mass comprises predominantly (at least 80%) of the ester functions and terephthalic acid. The polyester yarn is lightweight and flexible. It is resistant to ultraviolet radiation. Low flammability. It softens at 245 ° C and melts at 250 ° C. It keeps a good shape memory and can therefore be used into coated fabrics composition. Furthermore, a suitable weaving also allows good heat dissipation. The AEM, better known by its brand name Vamac® is one of the most employed rubbers for the manufacture of products submitted to high temperatures while maintaining good properties against oxygen, ozone and light.

Applications:

  • Expansion joints
  • lifting bags
Properties:
  • Heat resistant
  • Non-skid
  • UV resistance
  • Ozone Resistance

Information provided by COLMANT COATED FABRICS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 30 - 9030 - 90
Tensile Strength at Break 8.00 - 20.0 MPa1160 - 2900 psi
Elongation at Break 100 - 900 %100 - 900 %
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 140 °C284 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Descriptive Properties
IRHD Hardness30-90
Point Temperature-50 C° - 150°C
Warp breaking strength90 - 2000 daN/5cm
Warp elongation at break10% - 20%
Weft breaking strength80 - 1400 daN/5cm
Weft elongation at break10% - 20%
Weight per sqm90 - 1100

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOLMANT038 / 316088

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.