MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® M36 180°C (350°F) Curing Epoxy Matrix
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: HexPly® M36 is a high performance 180ºC cure matrix developed for aerospace and industrial markets. It can be used in a variety of production techniques (Resin Film Infusion (RFI), prepreg and semiprepreg) making it easy to process. When cured, HexPly® M36 becomes a tough composite with excellent hot/wet performance. Its low density contributes to increased weight savings, and the flexibility in curing gives potential for composite part cost savings.

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 81.0 MPa
Tensile Modulus 3.50 GPa
Compressive Yield Strength 146 MPa
Poissons Ratio 0.42
Fracture Toughness 0.900 MPa-m½
Shear Modulus 1.23 GPaCalculated
Toughness 190 JPer square meter
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 211 °CDMTA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexPly® M21 356°F (180°C) Curing Epoxy Matrix
Hexcel® HexPly® M20 266°F (130°C) Curing Epoxy Matrix
Hexcel® HexPly® M18/1 180°C Curing Epoxy Matrix
Hexcel® HexPly® M18 356°F (180°C) Curing Epoxy Matrix
Hexcel® HexPly® M14 248°F (120°C) Curing Epoxy Matrix

PHEXC176 / 98647

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.