MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Brandenburger Supratherm HT 4 High Temperature Insulation Material  (discontinued **)
Categories: Ceramic

Material Notes: This medium-compressed silicate fibre material can withstand high temperatures. Application temperatures range up to approx. 850 °C.

Information provided by Brandenburger Isoliertechnik GmbH&Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.800 g/cc0.0289 lb/in³
Water Absorption 85 %85 %24 hrs; DIN 53 495
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 5.00 MPa725 psiEN 63
Compressive Strength 15.0 MPa2180 psiEN ISO 604
 10.0 MPa
@Temperature 200 °C
1450 psi
@Temperature 392 °F
EN ISO 604
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.00 µm/m-°C
@Temperature 20.0 °C
3.89 µin/in-°F
@Temperature 68.0 °F
DIN 53752
Thermal Conductivity 0.0900 W/m-K0.625 BTU-in/hr-ft²-°FDIN 52 612
 0.110 W/m-K
@Temperature 200 °C
0.763 BTU-in/hr-ft²-°F
@Temperature 392 °F
DIN 52612
Maximum Service Temperature, Air 850 °C1560 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Brandenburger Supratherm H High Temperature Insulation Material
Brandenburger Flexline Insulation
Brandenburger Supratherm T High Temperature Insulation Material
Brandenburger Supratherm HT 175 High Temperature Insulation Material
Brandenburger BRA-GLA Special Grade

PBRAND14 / 27728

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.