MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LyondellBasell Moplen HP560Z Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade

Material Notes: Moplen HP560Z is a polypropylene homopolymer used for extrusion applications. Moplen HP560Z has a very high melt flow rate, a very narrow molecular weight distribution and is in pelletized form. Moplen HP560Z is produced using a non-phthalate Ziegler/Natta catalyst and is used for the production of meltblown nonwovens with outstanding barrier/filtration properties. Moplen HP560Z is also used for compounding applications. This grade is not intended for medical and pharmaceutical applications.

Availability: Africa-Middle East; Europe

Application: Absorption & Filtration; Color Concentrates; Hygiene Nonwoven; Nonwovens; Wipes/Tissues

Market: Compounding; Textile

Processing Method: Compounding; Continuous Filament/Spinning; Fibers; Melt Blown

Attribute: Controlled Rheology; Extremely High Flow; Homopolymer; Narrow Molecular Weight Distribution

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 1500 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1500 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9682 / 324617

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.