Unibar 350 is a special grade alloyed to achieve the properties, giving excellent wear resistance, strength & heat-treatment response, while still possessing reasonable machinability and producing a good surface finish. Noise and vibration damping are good in this grade. Unibar-350 can be hardened by conventional methods, to Rc 50 on the bar surface. Information provided by United Cast Bar Ltd. |
EN-1561-GJL-350 GG35; Meehanite GA350 |