MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Stratasys® Antero™ 840CN03 PEKK-based 3D Printing Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyketone; PEKK, Unreinforced

Material Notes: Antero™ 840CN03 is a PEKK-based FDM thermoplastic combining the excellent physical and mechanical qualities of PEKK with electrostatic dissipative (ESD) properties. It is filled 3% by weight with carbon nanotubes. Antero 840CN03 exhibits exceptional chemical and wear resistance, ultra-low outgassing properties and consistent ESD performance. ESD values range from 10e4 – 10e9 ohms per square inch. This makes the material particularly suitable for space and industrial applications where these qualities are critical.

Information provided by Stratasys.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.27 g/cc1.27 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 50.0 MPa7250 psiZX Orientation; ASTM D638
 65.0 MPa9430 psiXZ Orientation; ASTM D638
Tensile Strength, Yield 95.0 MPa13800 psiXZ Orientation; ASTM D638
Elongation at Break 1.8 %1.8 %ZX Orientation; ASTM D638
 6.0 %6.0 %XZ Orientation; ASTM D638
Elongation at Yield 4.4 %4.4 %XZ Orientation; ASTM D638
Modulus of Elasticity 3.01 GPa437 ksiZX Orientation; ASTM D638
 3.17 GPa460 ksiXZ Orientation; ASTM D638
Flexural Strength 70.0 MPa10200 psiZX Orientation; ASTM D790, Procedure A
 135 MPa
@Strain 5.0 %
19600 psi
@Strain 5.0 %
XZ Orientation; ASTM D790, Procedure A
Flexural Modulus 2.70 GPa392 ksiZX Orientation; ASTM D790, Procedure A
 3.24 GPa470 ksiXZ Orientation; ASTM D790, Procedure A
Flexural Strain at Break 2.4 %2.4 %ZX Orientation; ASTM D790, Procedure A
Compressive Yield Strength 100 MPa14500 psiXZ Orientation; ASTM D695
 105 MPa15200 psiZX Orientation; ASTM D695
Compressive Modulus 2.61 GPa379 ksiXZ Orientation; ASTM D695
 2.63 GPa381 ksiZX Orientation; ASTM D695
Izod Impact, Notched 0.280 J/cm0.525 ft-lb/inZX Orientation; ASTM D256, ASTM D4812
 0.480 J/cm0.899 ft-lb/inXZ Orientation; ASTM D256, ASTM D4812
Izod Impact, Unnotched 1.28 J/cm2.40 ft-lb/inZX Orientation; ASTM D256, ASTM D4812
 14.7 J/cm27.5 ft-lb/inXZ Orientation; ASTM D256, ASTM D4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 10000 - 1.00e+9 ohm-cm10000 - 1.00e+9 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear 50.0 µm/m-°C
@Temperature 40.0 - 140 °C
27.8 µin/in-°F
@Temperature 104 - 284 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 150 °C302 °FASTM D648 Method B
Deflection Temperature at 1.8 MPa (264 psi) 153 °C307 °FASTM D648 Method B
Glass Transition Temp, Tg 158 °C316 °FInflection Point; ASTM D7426

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSTRAS906 / 255801

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.