(Viewing data as-entered.
Click here
to return)
Wall Colmonoy COLMONOY® 22 Nickel Alloy With Tungsten Carbide
Categories:
Metal
;
Metal Matrix Composite
;
Nonferrous Metal
;
Nickel Alloy
Material Notes:
A harder version of Colmonoy 23A and 24, used to repair blow holes, flaws, chips, and cracks in cast iron parts. Can be finished with a file.
Method of Application:
Oxyacetylene, Fusewelder
Information provided by Wall Colmonoy Corporation.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
8.58
g/cc
Mechanical Properties
Original Value
Comments
Hardness, Rockwell C
28 - 33
Thermal Properties
Original Value
Comments
Melting Point
1925
°F
Component Elements Properties
Original Value
Comments
Boron, B
1.5 %
Carbon, C
0.020 %
Chromium, Cr
0.080 %
Iron, Fe
0.12 %
Nickel, Ni
94.88 %
As Balance
Silicon, Si
3.4 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Wall Colmonoy COLMONOY® 21A PTA Nickel Alloy with Tungsten Carbide
Wall Colmonoy COLMONOY® 5 Hard-Surfacing Alloy Containing Wear-Resistant Chromium Borides and Carbides
Wall Colmonoy COLMONOY® 4 Hard-Surfacing Alloy With Chromium Boride
Wall Colmonoy COLMONOY® 23 Nickel Alloy With Tungsten Carbide
Wall Colmonoy COLMONOY® 24 Nickel Alloy With Tungsten Carbide
NWALL07 / 19774
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.