MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

AISI 4815H Steel, pseudocarburized, reheated to 830°C (1525°F) and oil quenched, 150°C (300°F) temper, 25 mm (1 in.) round
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 4000 Series Steel; Low Alloy Steel; Carbon Steel; Low Carbon Steel

Material Notes: Normalized 925°C (1700°F) in 32mm rounds, machined to 25 mm rounds, pseudocarburized at 925°C (1700°F) for 8 h., box cooled to RT, reheated to 830°C (1525°F), oil quenched, 150°C (300°F) temper, machined and tested in 12.8mm rounds.

Key Words: UNS H48150, ASTM A304, SAE J1268, low carbon steels
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.85 g/cc0.284 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 331331
Hardness, Knoop 359359Converted from Brinell
Hardness, Rockwell B 9999Converted from Brinell
Hardness, Rockwell C 3636Converted from Brinell
Hardness, Vickers 350350Converted from Brinell
Tensile Strength, Ultimate 1075 MPa155900 psi
Tensile Strength, Yield 910 MPa
@Strain 0.2 %
132000 psi
@Strain 0.2 %
Elongation at Break 15 %15 %in 50 mm.
Modulus of Elasticity 205 GPa29700 ksiTypical for steel
Bulk Modulus 160 GPa23200 ksiTypical for steel.
Poissons Ratio 0.290.29Calculated
Machinability 50 %50 %annealed and cold drawn. Based on 100% machinability for AISI 1212 steel.
Shear Modulus 80.0 GPa11600 ksiTypical for steel
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.0000260 ohm-cm
@Temperature 0.000 °C
0.0000260 ohm-cm
@Temperature 32.0 °F
condition of specimen unknown
 0.0000310 ohm-cm
@Temperature 100 °C
0.0000310 ohm-cm
@Temperature 212 °F
condition of specimen unknown
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.475 J/g-°C0.114 BTU/lb-°FTypical 4000 series steel
Thermal Conductivity 44.5 W/m-K309 BTU-in/hr-ft²-°FTypical steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.12 - 0.18 %0.12 - 0.18 %
Iron, Fe 94.645 - 96.03 %94.645 - 96.03 %As remainder
Manganese, Mn 0.30 - 0.70 %0.30 - 0.70 %
Molybdenum, Mo 0.20 - 0.30 %0.20 - 0.30 %
Nickel, Ni 3.2 - 3.8 %3.2 - 3.8 %
Phosphorus, P <= 0.035 %<= 0.035 %
Silicon, Si 0.15 - 0.30 %0.15 - 0.30 %
Sulfur, S <= 0.040 %<= 0.040 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 4817H Steel
AISI 4718H Steel, pseudocarburized, reheated to 850°C (1560°F) and oil quenched, 150°C (300°F) temper, 13.7 mm round
AISI 4815 Steel, pseudocarburized and oil quenched, 150°C (300°F) temper, 25 mm (1 in.) round
AISI 4815 Steel, pseudocarburized and oil quenched, 150°C (300°F) temper, 13.7 mm (1 in.) round
AISI 4720H Steel

M481AK / 7962

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.