MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lanxess Bayhibit® AM Plastic Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: BAYHIBIT® AM is a highly effective scale and corrosion inhibitor. Main field of application are the treatment of cooling and process water as well as the area of cleaning formulations.

Chemical composition: 50% solution of 2-Phosphonobutane-1,2,4-tricarboxylic acid (PBTC) in water

CAS-Reg.- No.: 37971-36-1

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 - 1.30 g/cc
Viscosity 10 - 25 cP
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
Appearanceclear, colorless to yellowish liquid
Color<100Hazen
Content<0.2%o-Phosphate
 <10 NTUTurbidity
 49-51%PBTC content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Oceanchem Group Melamine Polyphosphate (MPP)
Arkema LOTADER® AX 8900 Terpolymer Ethylene - Acrylic Ester - Glycidyl Methacrylate
Lanxess STABAXOL® KE 9193 Masterbatch Antihydrolysis agent
Lanxess Bayhibit® S Granulate Plastic Additive
Lanxess Bayhibit® N Plastic Additive

PLANY8383 / 208776

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.