MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Epoxies, Etc 40-3920 Electrically Conductive Flexible Ink
Categories: Other Engineering Material

Material Notes: Description: 40-3920 is a one component electrically conductive ink. 40-3920 is a silver filled polymer system which exhibits outstanding adhesion to a variety of substrates, such as kapton, mylar, glass, polyester, ceramic, etc. This thick film ink provides excellent conductivity for many electronic applications. It is screen printable and also sprayable.

Applications:

  • Membrane Switches
  • Flexible Circuits
  • Polymer Thick Film Circuits
  • EMI/RFI Shielding
Features:
  • Flexible
  • Low Electrical Resistance
  • Low viscosity
  • Excellent Adhesion

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.20 g/cc2.20 g/cc
Viscosity 9000 cP9000 cP
Storage Temperature 18.0 - 30.0 °C64.4 - 86.0 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000200 ohm-cm0.000200 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 140 °C284 °F
Minimum Service Temperature, Air -20.0 °C-4.00 °F
Flash Point 99.0 °C210 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  8.00 - 10.0 min
@Temperature 107 °C
0.133 - 0.167 hour
@Temperature 225 °F
 20.0 - 30.0 min
@Temperature 25.0 °C
0.333 - 0.500 hour
@Temperature 77.0 °F
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
ColorSilver

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFEPOX095 / 316772

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.