MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dura-Bar G2A Continuously Cast Gray Iron Bar Stock ASTM A48
Categories: Metal; Ferrous Metal; Cast Iron; Alloy Cast Iron; Gray Cast Iron

Material Notes: Dura-Bar G2A has Type D graphite in a predominantly pearlitic matrix. The fine graphite structure allows excellent surface finish and is normally used in permanent mold applications requiring optimal strengths and wear resistance.

The microstructure will contain Type VII, type D, size 6-8, graphite as defined in ASTM A247. The matrix is predominantly pearlite. The rim will be similar to the center. Chill carbides will be less than 5% in any field at 100x and will be well dispersed.

G2A Dura-Bar can be oil quench hardened from 1600F (870C) to a minimum hardness of 50 Rc on the outside of the bar. The inside diameter hardness will be less than 50 Rc. Lower quench hardnesses on the inside diameters are a result of larger graphite flakes and not a loss of matrix hardness.

Composition: Typical chemical composition and ranges, actual values depend on cross section size.

Information provided by Dura-Bar.

Vendors: Dura-Bar Metal Services is the leading supplier of Dura-BarĀ® continuous cast iron and a major distributor of bronze alloys. Our customers rely on us for high quality materials that help increase their profitability. Call us at 1-800-526-0548 or visit dura-barms.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 248 - 311
Tensile Strength, Ultimate 40000 psi
Shear Strength 30000 psi
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 2.6 - 3.75 %
Iron, Fe 92.7 - 95.2 %As Balance
Manganese, Mn 0.20 - 0.40 %
Phosphorus, P <= 0.12 %
Silicon, Si 2.0 - 3.0 %
Sulfur, S <= 0.02500 %
 
Descriptive Properties
Endurance Ratio0.5
Heat-Treat Response (Rc)55-60
Relative Damping Capacity250Natural log of rate of successive amplitude.
Relative Wear ResistanceFair

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dura-Bar G1 Continuously Cast Gray Iron Bar Stock ASTM A48
Dura-Bar G2 Continuously Cast Gray Iron Bar Stock ASTM A48
Dura-Bar G1A Continuously Cast Gray Iron Bar Stock ASTM A48
Gray Cast Iron, ASTM A 48 Class 40
ASTM class 35 Standard gray iron test bars, as cast

NDURA05B / 138286

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.