MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

BASF Ultradur® S 4090 GM11 5/5% Glass/Mineral Filled PBT + ASA
Categories: Polymer; Thermoplastic; ASA Polymer; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: PBT + ASA, injection-molding grades reinforced with 5% glass fiber/mineral, for laminar parts with high demands on dimensional stability and low warpage, e.g. lids, ventilation grilles and housing covers.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.29 g/cc0.0466 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.20 %0.20 %23°C; 50% RH
Water Absorption at Saturation 0.40 %0.40 %DIN 53495/1L
Viscosity Test 139 cm³/g1.39 dl/gViscosity number; ISO 1628
Linear Mold Shrinkage, Flow 0.010 cm/cm0.010 in/inSheet
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/inSheet
Melt Flow 14.19 g/10 min
@Load 2.16 kg,
Temperature 275 °C
14.19 g/10 min
@Load 4.76 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 63.0 MPa9140 psi50 mm/min; ISO 527-2
Elongation at Break 3.8 %3.8 %50mm/min; ISO 527-2
Modulus of Elasticity 4.00 GPa580 ksiISO 527-2
Flexural Strength 104 MPa15100 psiISO 178
Charpy Impact Unnotched 4.00 J/cm²19.0 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.450 J/cm²2.14 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 - 225 °C428 - 437 °FDSC; ISO 11357-3
Maximum Service Temperature, Air 170 °C338 °F
Deflection Temperature at 0.46 MPa (66 psi) 195 °C383 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 105 °C221 °FISO 75-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 275 °C482 - 527 °FInjection-molding
Mold Temperature 60.0 - 100 °C140 - 212 °F
 
Descriptive Properties
ColorNatural
Commercial StatusEurope
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultradur® S 4090 GM13 5/15% Glass/Mineral Filled PBT + ASA
BASF Ultradur® B 4406 G6 30% Glass Filled PBT
BASF Ultradur® B 4300 M2 12.5% Mineral Filled PBT
BASF Ultradur® B 4300 K6 30% Glass Bead Filled PBT
BASF Ultradur® B 4300 K4 20% Glass Bead Filled PBT

PBASG0108 / 131742

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.