MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
KLJ Group KLJ-XL-01 XLPE
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: KLJ-XL compounds are a combination of LLDPE base material and catalyst master batch. The base polymer LLDPE is grafted with Vinyl Silane. The process results in moisture/ambient curable polymer having excellent processing characteristics without any volatiles. When properly mixed, addition of 5 parts of corresponding catalyst materbatch to 95 parts of grafted polymer, an insulation with excellent thermo-oxidative stability is achieved.

Application: Grafted polymer & corresponding catalyst masterbatch of each grade is designed for insulation of low voltage (up to 6 KVA)/medium voltage (up to 33 KVA) application and power cables.

Specifications: Grafted polymer in combination with corresponding catalyst masterbatch meets the following specifications, when processed using sound extrusion practice and testing procedures.

IEC-60502, IS-7098 (Part-I & II), IS 3396

Information provided by KLJ Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Deformation <= 2.5 %IS 10810 Part 30/IEC 60502
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 20.0 MPaIS 10810 Part 7/IEC 60502
 >= 21.6 MPa
@Treatment Temp. 132 - 138 °C,
Time 605000 sec
IS 10810 Part 11/IEC 60502
Elongation at Break >= 600 %IS 10810 Part 7/IEC 60502
 >= 300 %
@Treatment Temp. -30.0 °C
Cold Elongation Test; IS 10810 Part 11
 >= 558 %
@Treatment Temp. 132 - 138 °C,
Time 605000 sec
IS 10810 Part 11/IEC 60502
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 2.50e+16 ohm-cmIS 3396
Dielectric Constant <= 1.7IEC 60250
Dielectric Strength >= 30.0 kV/mmIEC 60243
Dissipation Factor <= 0.00020IEC 60250
 
Thermal PropertiesOriginal ValueComments
Shrinkage <= 1.2 %
@Temperature 127 - 133 °C,
Time 3600 sec
IS 10810 Part 30/IEC 60502
 
Processing PropertiesOriginal ValueComments
Zone 1 115 - 145 °C
Zone 2 135 - 165 °C
Zone 3 155 - 185 °C
Zone 4 175 - 205 °C
Zone 5 185 - 215 °C
Die Temperature 190 - 220 °C
Head Temperature 190 - 220 °C
Shelf Life 6.00 Month
 
Descriptive Properties
Content600 ppmMoisture
Hot Set<70%200°C/15 minute 20N/cm2 (Thickness 1.0 mm), IS 18010 Part-30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKLJ215 / 284236

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.