MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
ASTM A710 Steel, grade A, class 1, 8 - 19 mm inclusive
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; ASTM Steel; Carbon Steel; Low Carbon Steel

Material Notes: Low-carbon age-hardened alloy steel

Precipitation heat treated at 540 - 650°C. The following are suggested consumables for arc welding processes: Manual Shielded Metal-Arc (AWS A5.5) Low Hydrogen Electrodes E9016, and E9018; Submerged Arc (AWS A5.23) F9x-Exxx; Gas Metal-Arc (AWS A5.28) ER90S-x; Flux Cored-Arc (AWS A5.29) E9xT-x except -2, -3, -10, and -GS.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 620 MPa
Tensile Strength, Yield 550 MPa
Elongation at Break 20 %
Modulus of Elasticity 205 GPaTypical for steel
Bulk Modulus 160 GPaTypical for steel
Poissons Ratio 0.29Calculated
Shear Modulus 80.0 GPaTypical for steel.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000234 ohm-cmTypical steel
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.475 J/g-°CTypical steel
Thermal Conductivity 46.6 W/m-KTypical steel
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.070 %
Chromium, Cr 0.60 - 0.90 %
Copper, Cu 1.0 - 1.3 %
Iron, Fe 95.33 - 97.13 %As remainder
Manganese, Mn 0.40 - 0.70 %
Molybdenum, Mo 0.15 - 0.25 %
Nickel, Ni 0.70 - 1.0 %
Niobium, Nb (Columbium, Cb) >= 0.020 %
Phosphorus, P <= 0.025 %
Silicon, Si <= 0.40 %
Sulfur, S <= 0.025 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ASTM A710 Steel, grade A, class 2, 6.4 - 25 mm inclusive
ASTM A514 Steel, grade P, plate thickness ≤ 19 mm
ASTM A516 Carbon Steel, Grade 70
ASTM A710 Steel, grade A, class 3, thickness > 50 mm
ASTM A710 Steel, grade A, class 2, 25 - 50 mm inclusive

M710AA / 8260

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.