Petrothene LT602902 is a high density polyethylene sheet extrusion grade with excellent extrusion characteristics and low warpage. The resulting sheet exhibits good stiffness and impact properties. Typical applications include sheet for signage and packaging. Availability: North America Application: General Sheet Extrusion; Housewares; Structural Parts Market: Rigid Packaging Processing Method: Extrusion Blow Molding; Sheet and Profile Extrusion Attribute: Good Processability Information provided by LyondellBasell. |