MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
AISI Type 304L Stainless Steel
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Austenitic Cr-Ni stainless steel. Better corrosion resistance than Type 302. High ductility, excellent drawing, forming, and spinning properties. Essentially non-magnetic, becomes slightly magnetic when cold worked. Low carbon content means less carbide precipitation in the heat-affected zone during welding and a lower susceptibility to intergranular corrosion. Applications include beer barrels, bellows, chemical equipment, coal hopper linings, cooling coils, cryogenic vessels, dairy equipment, evaporators, feedwater tubing, flexible metal hose, food processing equipment, hypodermic needles, nuclear vessels, oil well filter screens, refrigeration equipment, paper industry, pressure vessels, sanitary fittings, valves, shipping drums, spinning, still tubes, textile dyeing equipment, tubing.

Key Words: aisi304, AISI 304, T304, T 304, SUS304, SS304, 304SS, 304 SS, T304L, T304 L, 304L, 304 L, UNS S30403, AMS 5647, QQ-S-763, austenitic, Cr-Ni stainless steel, SAE 30304L, DIN 1.4306, X2CrNi189, B.S. 304 S 12, PN 86020 (Poland), OOH18N10, ISO 4954 X2CrNi1810E, ISO 683/13 10, 18-8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop 158Converted from Rockwell B Hardness Value
Hardness, Rockwell B 82
Hardness, Rockwell C 1510% Cold-worked
Hardness, Vickers 159Converted from Rockwell B Hardness Value.
Tensile Strength, Ultimate 564 MPa0% Cold-worked
Tensile Strength, Yield 210 MPa0% Cold-worked
Elongation at Break 58 %In 50mm (2 in.)
Modulus of Elasticity 193 - 200 GPa
Charpy Impact 216 J
 
Electrical PropertiesOriginal ValueComments
Magnetic Permeability 1.008at RT
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.500 J/g-°CEstimated based on a comparison with similar stainless steels.
Thermal Conductivity 97.0 - 113 BTU-in/hr-ft²-°F
Melting Point 1400 - 1450 °C
Solidus 1400 °C
Liquidus 1450 °C
Maximum Service Temperature, Air 870 °CIntermittent
 925 °CContinuous Service
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.030 %
Chromium, Cr 18 - 20 %
Iron, Fe 64.9 - 74 %as balance
Manganese, Mn <= 2.0 %
Nickel, Ni 8.0 - 12 %
Phosphorus, P <= 0.045 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
304 Stainless Steel
AISI Type 316L Stainless Steel, annealed sheet
AISI Type 304L Stainless Steel, Annealed Bar, Longitudinal
AISI Type 304HN Stainless Steel
316 Stainless Steel, annealed sheet

MQ304L / 12676

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.