MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Elmet Technologies ET92.5NM Tungsten Heavy Alloy
Categories: Metal; Nonferrous Metal; Refractory Metal; Tungsten Alloy

Material Notes: Elmet Technologies presses and sinters high quality tungsten heavy alloy (WHA) blocks, rods, and shaped parts. All material is made in the USA at Elmet’s fully integrated facility in Lewiston, Maine. Elmet has a large and growing inventory of standard molds and sizes that can be sold “rough as sintered” or machined to provide tighter tolerances. Sintered WHA blanks can be further rolled or swaged by Elmet to produce plates, sheets, and rods. Elmet also precision machines WHA parts for use as ballast weights, radiation shields, boring bars, ordnance components, and other components that require high density and good ductility.

Information provided by Elmet Technologies.

Key Words: WNiFe Class 2; Tungsten Heavy Alloy WHA
Vendors: Elmet Technologies is a 100% US owned and operated, fully integrated manufacturer of Molybdenum, Tungsten and related alloys such as TZM, WHA & MoLa. At our 220,000 sqr/ft plant in Lewiston, Maine, Elmet manufactures W & Mo pure powders plus rod, wire, plate, sheet & foil in additional to offering fabrication and machining services. ITAR, ISO and AS9100 registered. www.elmettechnologies.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 17.5 g/cc0.632 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C <= 33<= 33
Tensile Strength, Ultimate >= 648 MPa>= 94000 psi
Tensile Strength, Yield >= 517 MPa>= 75000 psi
Elongation at Break >= 2.0 %>= 2.0 %
 
Electrical PropertiesMetricEnglishComments
Magnetic Permeability <= 1.05<= 1.05
 
Component Elements PropertiesMetricEnglishComments
Iron, Fe 0.80 %0.80 %
Nickel, Ni 6.7 %6.7 %
Tungsten, W 92.5 %92.5 %
 
Descriptive Properties
AMS 7725EClass 2, Type 1
ASTM B-777Class 2
MIL-T-21014DClass 2
REACH ComplianceRegulation (EC) No. 1907/2006
RoHS Compliance2002/95/EC, 2011/65/EU
WHA Block - Ground Finish Sizes1.50"T X 4.75"W X 7.25"LTolerances: +/-0.030"; Class 1: 14.39 kg
 1.50"T X 4.750"W X 4.50"LTolerances: +/-0.030"; Class 1: 8.93 kg
 1.65"T X 1.7"W X 6.0"LTolerances: +/-0.030"; Class 1: 4.69 kg
 2.10"T X 2.375"W X 7.0"LTolerances: +/-0.030"; Class 1: 9.72 kg
 2.20"T X 3.2"W X 5.0"LTolerances: +/-0.030"; Class 1: 9.8 kg
 2.25"T X 4.75"W X 4.0"LTolerances: +/-0.030"; Class 1: 11.91 kg
 2.25"T X 4.75"W X 5.0"LTolerances: +/-0.030"; Class 1: 14.88 kg
 2.25"T X 4.75"W X 6.0"LTolerances: +/-0.030"; Class 1: 17.86 kg
 2.875"T X 4.0"W X 6.0"LTolerances: +/-0.030"; Class 1: 19.22 kg
WHA Block - Rough As Sintered Sizes1.60"T X 4.875"W X 4.625"LTolerances: +/- 3/16"; Class 1: 10 kg
 1.60"T X 4.875"W X 7.5"LTolerances: +/- 3/16"; Class 1: 16.5 kg
 1.75"T X 1.8"W X 6.2"LTolerances: +/- 3/16"; Class 1: 5.5 kg
 2.20"T X 2.5"W X 7.2"LTolerances: +/- 3/16"; Class 1: 11.25 kg
 2.30"T X 3.3"W X 5.2"LTolerances: +/- 3/16"; Class 1: 11 kg
 2.375"T X 4.9"W X 4.2"LTolerances: +/- 3/16"; Class 1: 13.75 kg
 2.375"T X 4.9"W X 5.2"LTolerances: +/- 3/16"; Class 1: 17 kg
 2.375"T X 4.9"W X 6.2"LTolerances: +/- 3/16"; Class 1: 20.5 kg
 3.0"T X 4.125"W X 6.2"LTolerances: +/- 3/16"; Class 1: 21.5 kg
WHA Round - Rough As Sintered Sizes0.720" X 12.20"Diameter Tolerance: +/-0.030"; Length Tolerance: +/-0.125"
 0.950" X 12.20"Diameter Tolerance: +/-0.060"; Length Tolerance: +/-0.125"
 1.30" X 12.20"Diameter Tolerance: +/-0.075"; Length Tolerance: +/-0.125"
 1.62" x 12.20"Diameter Tolerance: +/-0.075"; Length Tolerance: +/-0.125"
 1.90" X 12.20"Diameter Tolerance: +/-0.075"; Length Tolerance: +/-0.125"
 2.10" X 12.20"Diameter Tolerance: +/-0.090"; Length Tolerance: +/-0.125"
 2.95" X 6.25"Diameter Tolerance: +/-0.125"; Length Tolerance: +/-0.125"
WHA Round Turned Finish Sizes0.625" X 12"Diameter Tolerance:+0.015"-0.005"; Length Tolerance: +0.125"-000
 0.875" X 12"Diameter Tolerance:+0.015"-0.010"; Length Tolerance: +0.125"-000
 1.125" X 12"Diameter Tolerance:+0.030"-0.010"; Length Tolerance: +0.125"-000
 1.50" x 12"Diameter Tolerance:+0.030"-0.010"; Length Tolerance: +0.125"-000
 1.75" X 12"Diameter Tolerance:+0.030"-0.010"; Length Tolerance: +0.125"-000
 2.00" X 12"Diameter Tolerance:+0.030"-0.010"; Length Tolerance: +0.125"-000
 2.75" X 6"Diameter Tolerance:+/-0.030"; Length Tolerance: +0.125"-000

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NELMET903 / 242024

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.