MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Lucas-Milhaupt Silvaloy® 580 Silver Based Cadmium Free Filler Metal
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Braze 580 is a free flowing intermediate temperature cadmium-free silver brazing filler metal that exhibits an unusual ability to wet certain base metals that are difficult to braze with more standard alloys. Typical of these base metals are chromium and tungsten carbides. Unlike some other manganese containing brazing filler metals, Braze 580 does not tend to produce porous fillets. Braze 580 contains no zinc or cadmium and will not outgas during Titanium Nitride coating of tools.

Applications:This alloy should be regarded as a special purpose material for brazing difficult to wet metals and alloys such as tungsten and chromium carbides. Wetting studies show that this alloy exhibits excellent wetting in vacuum brazing of high manganese stainless steels. For details consult: Vacuum Brazing of High Manganese Stainless Steel by W. S. Bennett and R.F. Hillyer, Welding Journal (Vol 53, No. 11, Nov. 1974, P510S).

Information provided by Lucas-Milhaupt, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 9.82 g/cc
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000681 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Melting Point 1120 - 1345 °F
Solidus 1120 °FMelting Point
Liquidus 1345 °FFlow Point
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 31.5 - 33.5 %
Manganese, Mn 2.5 - 3.5 %
Other, total <= 0.15 %
Silver, Ag 56.5 - 58.5 %
Tin, Sn 6.5 - 7.5 %
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bisalloy Steels BisPlate 400 Thickness >80-100 mm
Lucas-Milhaupt Silvaloy® 603 Silver Based Cadmium Free Filler Metal
Lucas-Milhaupt Silvaloy® 650 (Easy) Silver Based Cadmium Free Filler Metal
DP-3 Duplex Stainless Steel (UNS S31260)
Carlson 2205 (UNS S31803) Duplex Stainless Steel

NLUCMI25 / 18092

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.