MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Evonik VESTOPLAST® EP 807 Amorphous Polyalphaolefin
Categories: Polymer; Thermoplastic; Polyalphaolefin

Material Notes: Amorphous Poly-alpha-olefins: With its VESTOPLASTR amorphous poly-alpha-olefins (APAO) Evonik offers a broad range of co- and terpolymers of ethene, propene and 1-butene as raw materials for various applications. Under variation of monomer composition, molecular weight and chemical modification optimum values are achieved for properties like hardness, melt viscosity, crystallinity and rate of crystallization. The production process allows us to offer both predominately amorphous, soft grades as well as harder, partially crystalline grades. In addition to our regular, pure thermoplastic grades we also offer unique reactive, silane-modified amorphous poly-alpha-olefins like VESTOPLASTR 206. VESTOPLASTR is usually supplied as granules in 20 kg polyethylene bags. A special wax powdering technique improves the flowability of the material. Your benefits:
  • excellent adhesion and hot tack properties
  • bonding to various substrates
  • good cohesion and high thermal stability
  • good moisture and gas barrier behaviour
  • very good hydrolytic and UV stability

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 5000 - 9000 cPDIN 53019
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 4.00 MPaDIN EN ISO 527-3
Elongation at Break 40 %DIN EN ISO 527-3
 
Thermal PropertiesOriginal ValueComments
Softening Point 158 - 164 °CDIN EN 1427
Glass Transition Temp, Tg -28.0 °CDIN 53 765

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik VESTOPLAST® 206 + 6%, 206 B Amorphous Polyalphaolefin
Evonik VESTOPLAST® EP NC 702 Amorphous Polyalphaolefin
Evonik VESTOPLAST® 708 Amorphous Polyalphaolefin
Evonik VESTOPLAST® 704 Amorphous Polyalphaolefin
Evonik VESTOPLAST® 703 Amorphous Polyalphaolefin

PEVONIL123 / 196327

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.