MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ITW Plexus Plexus™ MA1023 Methacrylate Adhesive  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.

Low shrinkage, low odor, all purpose.

Information provided by Illinois Tool Works.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.23 lb/galMixed
Viscosity 50000 - 70000 cPB
 150000 - 175000 cPA
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 1750 - 2000 psi
Elongation at Break 100 - 125 %
Tensile Modulus 60000 - 80000 psi
Shear Strength 1400 - 1600 psi
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -67.0 °F
Flash Point 51.0 °FTCC
 
Processing PropertiesOriginal ValueComments
Pot Life 7.0 - 8.0 min
 
Descriptive Properties
ColorOff-white, Blue
Fixture Time20-25 minutes
Gap FillingMax 0.375 in
Mix Ratio10:1By volume

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ITW Plexus Plexus™ MA420FS Methacrylate Adhesive
ITW Plexus Plexus™ MA1021 Methacrylate Adhesive
Evonik Rohacell® P 170 Polymethacrylimide (PMI) Rigid Foam Sheet
Evonik Rohacell® 200 WF High Heat Grade Polymethacrylimide (PMI) Foam

PMM9022 / 53332

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.