MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Ineos G60-25-144 HDPE  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Ineos G60-25-144 is a high density polyethylene homopolymer typically used in the production of sheet extrusion and blow molded containers. This material meets the Food and Drug Administration requirements of 21CFR 177.1520.

Key Words: Sheet extrusion and blow molded containers
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.962 g/cc0.0348 lb/in³ASTM D4883
Melt Flow 0.25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.25 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6666ASTM D2240
Tensile Strength, Yield 31.0 MPa4500 psi2 in/min (50 mm/min); ASTM D-638
Elongation at Break >= 800 %>= 800 %2 in/min (50 mm/min); ASTM D-638
Modulus of Elasticity 1.344 GPa194.9 ksiASTM D638
Flexural Modulus 0.861 GPa125 ksiASTM D747
 1.55 GPa225 ksiTangent-Method 1; ASTM D790
Izod Impact, Notched 2.10 J/cm3.93 ft-lb/inASTM D256
Tensile Impact Strength 258 kJ/m²123 ft-lb/in²Type L, ASTM D1822
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C176 °FASTM D648
Vicat Softening Point 131 °C268 °FASTM D1525
Brittleness Temperature <= -75.0 °C<= -103 °FASTM D746
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
processBlow Molding
 Sheet Extrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos TC46-25 HDPE
Ineos A60-70-162 HDPE
Ineos K44-11-128 HDPE
Ineos T60-1200-119 HDPE
Huntsman PE7076 Profile Extrusion Polyethylene

PSOLJC / 68182

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.