MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Phillips 66 Kendall® SHP® Diesel Engine Oil SAE Grade 5W-40
Categories: Fluid; Lubricant

Material Notes: Kendall® SHP Diesel Full Synthetic Engine Oil is a premium quality, full-synthetic engine oil developed for use in four-stroke cycle diesel engines operating under extreme temperature conditions. It meets API CJ-4 performance requirements for use in modern low-emission engines designed to meet 2007 and later EPA on-highway exhaust emissions standards, and is backward serviceable for use in older diesel engines. It is specially formulated for compatibility with exhaust aftertreatment systems using diesel particulate filters (DPF), diesel oxidation catalysts (DOC) and/or selective catalytic reduction (SCR). The full-synthetic formulation and SAE 5W-40 viscosity grade provide excellent low-temperature properties for better performance in harsh winter climates. SHP Diesel Full Synthetic is formulated with synthetic base stocks and an advanced low-SAPS additive package to provide outstanding wear protection, soot control and bearing corrosion protection in both conventional and EGR-equipped diesel engines. It has excellent soot dispersancy to protect against abrasive wear and soot-induced oil thickening, and to ensure good low-temperature pumpability even with highly soot-laden oil. The full-synthetic formulation provides enhanced oxidation resistance and thermal stability at high temperatures and improved low-temperature properties compared with a conventional, non-synthetic formulation. SHP Diesel Full Synthetic meets or exceeds the performance requirements of API Service Categories CJ-4 and SN, and is approved under the latest OEM specifications for use in low-emission diesel engines. It is backward serviceable for use where earlier API “C” category engine oils, or the concurrent earlier OEM specifications, are specified. It is formulated for use in diesel engines operating on diesel fuels with sulfur content up to 500 ppm. However, for applications not using Ultra-Low Sulfur Diesel (ULSD), consult the engine manufacturer for recommended service interval.

Applications:

  • On- and off-highway diesel equipment operating at low ambient temperatures
  • On-highway diesel trucks equipped with EGR and exhaust aftertreatment systems to meet 2007/2010 emissions standards
  • Older diesel equipment with conventional, non-EGR engines or ACERT engines
  • Off-highway construction, earth moving and mining equipment
  • Mixed fleets with diesel and gasoline-fueled vehicles
SHP Diesel Full Synthetic is licensed or OEM-certified for:
  • API Service CJ-4, CI-4 with CI-4 PLUS, CI-4, CH-4, SN
  • Cummins CES 20081
  • Detroit Diesel Power Guard 93K218
  • Mack EO-O Premium Plus
  • Mercedes-Benz Sheet 228.31
  • Volvo VDS-4
SHP Diesel Full Synthetic meets or exceeds the requirements of:
  • ACEA E9-08, E7-08
  • Caterpillar ECF-3, ECF-2, ECF-1-a
  • Deutz DQC III-05
  • Ford WSS-M2C171-E
  • Renault VI RLD-3
  • Diesel engines manufactured by OEMs not listed above, where the OEM specifies API CJ-4 engine oil
Features/Benefits:
  • Excellent protection for newer low-emission diesel engines and older diesel engines
  • Specially formulated to protect exhaust aftertreatment systems
  • Outstanding soot control for protection against abrasive wear and soot-induced oil thickening
  • Outstanding resistance to viscosity and thermal breakdown at high temperatures
  • Protects against sludge and varnish formation
  • Protects against rust, bearing corrosion and wear
  • Excellent low-temperature pumpability for easier starting and less wear during cold starts
  • High shear stability
  • Good resistance to foaming and aeration

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.853 g/cc
Density 7.10 lb/gal
Viscosity 4.2 cP
@Temperature 150 °C
High-Temp/High-Shear
 6250 cP
@Temperature -30.0 °C
Cold-Cranking
Viscosity Measurement 166Index
Kinematic Viscosity at 40°C (104°F) 95 cSt
Kinematic Viscosity at 100°C (212°F) 15.1 cSt
Ash 1.0 %Sulfated; ASTM D874
ASTM Color 4.0ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Base Number 9.3ASTM D2896
 
Thermal PropertiesOriginal ValueComments
Pour Point -48.0 °C
Flash Point 240 °CCOC
 
Component Elements PropertiesOriginal ValueComments
Zinc, Zn 0.132 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5299 / 198552

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.