MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil Mobil 1 75W-90 Gear Lubricant LS
Categories: Fluid; Lubricant

Material Notes: Mobil 1 Synthetic Gear Lubricant LS is a supreme performance, synthetic, multi-purpose, SAE 75W-90 automotive gear lubricant designed to meet the highest level performance requirements of modern passenger vehicles in all types of operating conditions including limited slip applications, as well as, deliver outstanding power transfer performance. Compared to conventional hypoid gear lubricants, Mobil 1 Synthetic Gear Lubricants LS 75W-90 performs exceptionally over a wide range of temperatures. Mobil 1 Synthetic Gear Lubricant LS 75W-90 achieves this through a unique proprietary formulation, that deliver optimized viscosity-temperature properties together with the highest level of inherent formulation stability and protects against thermal and oxidative degradation, wear and corrosion, viscosity loss associated with premature shearing. It also can be used in extended service and for aiding in fuel economy performance. Mobil 1 Synthetic Gear Lubricant LS 75W-90 meets the most severe API Service MT-1 and GL-5 EP gear oil service classification.

Mobil 1 Synthetic Gear Lubricant LS 75W-90 is recommended for use in modern high performance automobiles like SUVs, Vans and Light duty trucks requiring API GL-5 and MT-1 level performance; Mobil 1 Synthetic gear Lubricant LS 75W-90 is intended for initial fill, topping-off or refilling differentials, final drives, transfer cases and other gear applications where lubricants meeting API Service GL-5 and multi-purpose or mild EP gear lubricants are recommended; Mobil 1 Synthetic Gear Lubricant LS 75W-90 can also be used in rear axles where API Service GL-4 lubricant is recommended; Not recommended for automatic, manual or semiautomatic transmissions for which engine oil or automatic transmission fluids are recommended; Where extended service intervals and warranties are required

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.859 g/cc
@Temperature 15.0 °C
0.0310 lb/in³
@Temperature 59.0 °F
ASTM D4052
Viscosity Measurement 150150Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 106 cSt106 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 15.2 cSt15.2 cStASTM D445
 
Thermal PropertiesMetricEnglishComments
Pour Point -46.0 °C-50.8 °FASTM D97
Flash Point 175 °C347 °FASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WEXXON051 / 75476

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.