MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Rogers Arlon R37230R006 0.006" (0.152 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Substrate
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Design/Construction:
Liner: FEP
Add-on: Uncured Silicone Rubber
Substrate: PTFE Coated Fiberglass

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³Silicone Property; Arlon SQA-TMS-024
Thickness 25.4 microns1.00 mil
 152 microns6.00 milOverall; Arlon SQA-TMS-003
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 1818Silicone Property; ASTM D2240
Tensile Strength 6.89 MPa1000 psiSilicone Property; ASTM D412
Elongation at Break 950 %950 %Silicone Property; ASTM D412
Modulus of Elasticity 0.000517 GPa0.0750 ksiSilicone Property; ASTM E 831
Poissons Ratio 0.500.50Approximately, Silicone Property
Shear Strength 3.96 MPa575 psiArlon SQA-TMS-018
 
Thermal PropertiesMetricEnglishComments
CTE, linear 335 µm/m-°C186 µin/in-°FSilicone Property; ASTM E 831
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°FSilicone Property; Arlon SQA-TMS-022
Maximum Service Temperature, Air 204.0 °C399.2 °F
Minimum Service Temperature, Air -136 °C-212 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 min
@Pressure 0.103 - 0.345 MPa,
Temperature 121 °C
0.250 hour
@Pressure 15.0 - 50.0 psi,
Temperature 250 °F
Recommended Cure Cycle
Shelf Life 6.00 Month
@Temperature 4.00 - 10.0 °C
6.00 Month
@Temperature 39.2 - 50.0 °F
From date of manufacture
 
Descriptive Properties
ColorRed
Total Product Weight (g/m2)175Arlon SQA-TMS-025

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Arlon R34332X039 0.039" (0.991 mm) Fully Cured/Unsupported
Parker Chomerics SOFT-SHIELD® 4800 Multi-planar EMI Gasket
Overview of materials for Silicone Rubber
Natural Rubber, Vulcanized (NR, IR, Polyisoprene)
Natural Rubber, Not Vulcanized (NR, IR, Polyisoprene)

PARL660 / 125846

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.