MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Matexcel NAT-1520 Nano Cellulose Powder
Categories: Wood and Natural Products

Material Notes: Cellulose nanofibers are high-purity plant cellulose nanofibers obtained by adopting a new environmentally friendly process under mild conditions. The preparation process has less waste water discharge and belongs to a clean green pulping process. In the liquid state, the nanofibers agglomerate during the drying process, and the size of the obtained dry powder becomes larger. The application fields of cellulose nanofibers involve biomedicine, automobile manufacturing, aerospace, construction, military special materials, electronic products, cosmetics, coatings, paints, food, paper, composite materials and polymer reinforcement, etc.

NAT-1520; Nano Cellulose Powder

Application: Biomedical, automotive, aerospace, construction, military materials, electronics, cosmetics, coatings, paints, food, paper, composite reinforcement

Morphology: White Powder

Key Words: Synonyms: Nano Cellulose Powder
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Filament Diameter 0.010 - 0.050 µm0.010 - 0.050 µmLength: 100-500nm
 
Descriptive Properties
Purity, %99.9%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMXCK1970 / 300601

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.