MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Chemours Viton® TBR-605CS with 30 phr Wollastocoat 10222  (discontinued **)
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Viton® Extreme™ TBR-605CS (formerly VTR-8802) is a base-resistant TFE/propylene polymer, containing a proprietary bisphenol curative. Viton® Extreme™ TBR-605CS utilizes a bisphenol cure site, together with optimized molecular architecture, to provide a polymer that:
  • Cures quickly, to a high state of cure
  • Exhibits excellent mold release and low mold fouling
  • Is inherently resistant to attack by basic chemicals
  • Provides excellent heat resistance
  • Provides superior resistance to hydrocarbon oils compared to other TFE-propylene polymers
  • Provides excellent compression set resistance

Information provided by manufacturer.

Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015. This specific grade had been discontinued prior to the spinoff.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7171Cured 10 min at 177°C and Post Cured 16 hr at 200°C
Tensile Strength, Ultimate 12.0 MPa1740 psiCured 10 min at 177°C and Post Cured 16 hr at 200°C
Elongation at Break 210 %210 %Cured 10 min at 177°C and Post Cured 16 hr at 200°C
100% Modulus 8.50 MPa
@Strain 100 %
1230 psi
@Strain 100 %
Cured 10 min at 177°C and Post Cured 16 hr at 200°C
Compression Set 31 %
@Temperature 200 °C
31 %
@Temperature 392 °F
Method B, O-rings, 70 hr
 
Descriptive Properties
Formulation as Tested100Viton® Extreme™ TBR-605CS
 30Wollastocoat 10222
 8High-Activity MgO

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Freudenberg V60 Standard Fluoroelastomer

PDVDA40 / 34009

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.