MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

H.C. Starck Grade UF 25 Silicon Carbide, SiC
Categories: Ceramic; Carbide

Material Notes: Alpha SiC for sintering.
  • Sliding bearings
  • Seal rings
  • Wear parts
  • Kiln furniture, crucibles, heating elements, burner nozzles, heat exchangers
  • Semiconductor handling parts
  • Components for wafer processing (susceptors, chucks, carriers)
  • electronic applications (varistors, diodes)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 0.45 µm0.45 µmAverage Particle Size/Laser Diffraction D50
Specific Surface Area 23 - 26 m²/g23 - 26 m²/gBET

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Silicon Carbide, Alpha SiC
H.C. Starck Grade UF 10 Silicon Carbide, SiC
H.C. Starck Grade UF 15 Silicon Carbide, SiC
Silicon Carbide, CVD
Silicon Carbide, sublimed

CHCSTA017 / 1195

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.