MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zinc ILZRO 16 (Zn-1.25Cu-0.2Ti-0.15Cr), Die Cast
Categories: Metal; Nonferrous Metal; Zinc Alloy

Material Notes: Conflicting reports about specified composition (Some omit aluminum). Recommended Casting Temperature 465°C

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.10 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 76500 kg load; 10 mm hardened steel ball
Hardness, Knoop 99Estimated from Brinell Value
Hardness, Vickers 86Estimated from Brinell Value
Tensile Strength, Ultimate 230 MPa
Tensile Strength, Yield 140 MPa0.2% Offset
Elongation at Break 6.0 %in 5 cm
Modulus of Elasticity 97.0 GPa
Charpy Impact, Unnotched 25.0 J
@Thickness 6.35 mm
square bar
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000840 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 27.0 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.402 J/g-°C
Thermal Conductivity 104.7 W/m-K
Melting Point 415 - 417 °C
Solidus 415 °C
Liquidus 417 °C
 
Processing PropertiesOriginal ValueComments
Casting Temperature 460 - 470 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.010 - 0.040 %
Cadmium, Cd <= 0.0040 %
Chromium, Cr 0.10 - 0.20 %
Copper, Cu 1.0 - 1.5 %
Iron, Fe <= 0.040 %
Lead, Pb <= 0.0050 %
Magnesium, Mg <= 0.020 %
Tin, Sn <= 0.0030 %
Titanium, Ti 0.15 - 0.25 %
Zinc, Zn 97.938 - 98.74 %As balance

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zinc ZA-12 (Zn-11Al-1Cu-0.025Mg), Die Cast
Zinc AC43A (Zinc Alloy 2; Zn-4Al-2.5Cu-0.04Mg; Number 2 Die Casting Alloy; Zamak 2), Die Cast
Zinc ZA-27 (Zn-27Al-2Cu-0.015Mg), Die Cast
Zinc ZA-8 (Zn-8Al-1Cu-0.02Mg), Die Cast
Zinc ZA-12 (Zn-11Al-1Cu-0.025Mg), Permanent Mold Cast

MZN160 / 14519

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.