MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Aluminum 7075-T76; 7075-T7651
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 7000 Series Aluminum Alloy

Key Words: UNS A97075; AA7075-T7651; Al7075-T7651
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 2.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate >= 503 MPaSheet
 >= 490 MPa
@Thickness 12.7 - 25.4 mm
Plate; T7651
 >= 496 MPa
@Thickness 6.35 - 12.7 mm
Plate; T7651
Tensile Strength, Yield >= 427 MPaSheet
 >= 414 MPa
@Thickness 12.7 - 25.4 mm
Plate; T7651
 >= 421 MPa
@Thickness 6.35 - 12.7 mm
Plate; T7651
Elongation at Break >= 8.0 %Sheet
 >= 6.0 %
@Thickness 12.7 - 25.4 mm
Plate; T7651
 >= 8.0 %
@Thickness 6.35 - 12.7 mm
Plate; T7651
Modulus of Elasticity 71.0 GPa
Compressive Modulus 72.4 GPa
Poissons Ratio <= 0.33
Shear Modulus 26.9 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000448 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.960 J/g-°C
Thermal Conductivity 150 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 87.1 - 91.4 %
Chromium, Cr 0.18 - 0.28 %
Copper, Cu 1.2 - 2.0 %
Iron, Fe <= 0.50 %
Magnesium, Mg 2.1 - 2.9 %
Manganese, Mn <= 0.30 %
Other, each <= 0.050 %
Other, total <= 0.15 %
Silicon, Si <= 0.40 %
Titanium, Ti <= 0.20 %
Zinc, Zn 5.1 - 6.1 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 7075-T6; 7075-T651
Aluminum 7075-T73; 7075-T735x
Aluminum 7075-O
Alclad Aluminum 7075-T6, T651
Aluminum 6061-T6; 6061-T651

MA7075T76 / 109186

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.