MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
LG Chemical LK170 PVC  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: General Description: LK170, vinyl chloride copolymer with vinyl acetate exhibit excellent properties including easy processing and effective flow

Main Applications: Sealant, automotive protective sol, carper under layer

CAS No: 9002-86-2 and 108-05-4

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.36 - 1.38 g/cc
Bulk Density 0.290 - 0.390 g/ccASTM D1895
Volatiles <= 1.5 %
@Temperature 110 °C,
Time 3600 sec
ASTM D3030-90
Brookfield Viscosity 5000 - 9000 cPDOP 60phr, 6RPM; ASTM D1824-90
Viscosity Measurement >= 1.0
@Pressure 0.400 MPa
[g/sec], DOP 60phr, Severs; ASTM D1823-90
 
Thermal PropertiesOriginal ValueComments
Flash Point 320 - 340 °C
Ignition Temperature 435 - 557 °CAutoignition
 
Descriptive Properties
Degree of Polymerization1550-165030°C, JIS K 6720-2
K-Value75DIN53726
VAc Contents2.5-4.5%ISO 1159

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Geon® Performance Solutions 130 Series 136 Polyvinyl Chloride Copolymer (PVC Copolymer)
Geon® Performance Solutions 130 Series 137 Polyvinyl Chloride Copolymer (PVC Copolymer)
Formosa Plastics Formolon® 113 PVC
Geon® Performance Solutions 130 Series 138 Polyvinyl Chloride Copolymer (PVC Copolymer)
Inovyn 460SL Polyvinyl Chloride grafted copolymer

PLAY710 / 148720

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.