MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Scotch® 214 High-Temperature Masking Tape
Categories: Polymer; Adhesive

Material Notes: Scotch® High Temperature Masking Tape 214 is good for one hour at 350°F (177°C) on most surfaces. The adhesive is sulfur-free which makes it one of the few tapes that can be used on copper, silver and other precious metals.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 0.174 milASTM D3652
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 32.7 MPaASTM D3759
Elongation at Break 10 %ASTM D3759
Peel Strength 1.8125 plito Steel; ASTM D3330
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 177 °C
 
Descriptive Properties
Adhesive TypeFirm rubber adhesive

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch® 232 High Performance Masking Tape
3M Scotch® 231A Performance Masking Tape
3M Scotch® 231 Performance Masking Tape
3M Scotch® 226 Solvent Resistant Masking Tape
3M Scotch® 222 High-temperature Fine Line Masking Tape

PMM34017 / 168764

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.